products 產品介紹

Free cutting Brass Rod & Wire

Nipple Using Brass:
Excellent Cold Forging And Good Machining.Use: Motorcycle and Bicycle Joint Nut.
Free Cutting Brass:
Excellent Machining and C3601,3602 with Good Extension too. Uses:Computer and Electronic, Clock, Pen, Light and Fishing Rivet: Nut, Gear, Valve Camera Parts, Hardware Parts. C3604, C3605
Forging Brass:
Excellent Hot Forging. Uses: Precision Forging, Machine Parts. Excellent Hot Forging And Good Machinability. Uses: Valve, Watch, Machine Parts.
Leadless Free Cutting Brass:
Leadless Free Cutting Brass Low Lead, low Cadmium, low Chromium, low Mercury suitable for Environment Purpose of Brass with Excellent Machinability. Use: Computer, Electronic, Clock, Pen, Light, Fishing, Rivet, Nut, Gear, Optical, Medical, Valve, Camera Parts and Hardware Parts.

Specialities and Utilities

Alloy No. Symbol Name Specialties and Utilities
C3501 wire(B)
#1.
Nipple Using Brass Excellent Cold Forging And Good Machining.
Use: Motorcycle and Bicycle Joint Nut.
C36000
C35300
C3601 (B)#1. Free Cutting Brass Excellent Machining and C3601,3602 with Good Extension too.
Uses:Computer and Electronic, Clock, Pen, Light and Fishing Rivet: Nut, Gear, Valve Camera Parts, Hardware Parts. C3604, C3605
C3602 (A)#1.
(B)#1.
C3603 (B)#1.
C3604 (A)#1.
(B)#1.
C3712 (A)#1. Forging Brass Excellent Hot Forging. Uses: Precision Forging, Machine Parts. Excellent Hot Forging And Good Machinability.
Uses: Valve, Watch, Machine Parts.
(B)#1.
C3771 (A)#1.
(B)#1.

#1. (A)Extrusion (B)Extrusion + Drawing

Composition

Copper Alloy CNS, JIS & ASTM No Composition(%)
Cu Pb Fe Fe+Sn Zn
C3501 60.0~64.0 0.7~1.7 0.20max 0.4max Rem
C3601 59.0~63.0 1.8~3.7 0.3max 0.5max Rem
C3602 59.0~63.0 1.8~3.7 0.5max 1.0max Rem
C3603 57.0~61.0 1.8~3.7 0.35max 0.6max Rem
C3604 57.0~61.0 1.8~3.7 0.5max 1.0max Rem
3712 58.0~62.0 0.25~1.2 0.8max Rem
3771 57.0~61.0 1.0~2.5 1.0max Rem
ASTM C36000 60.0-63.0 2.5-3.7 0.35max Rem
ASTM C35300 61.0-63.0 1.5-2.5 0.15max Rem
ASTM C38500 55.0~59.0 2.5~3.5 0.35max Rem
DIN CuZn39Pb3 57.0~59.0 2.5~3.5 0.30max Sn<0.3, Ni<0.3,Al<0.05 Rem
Hot Forging Brass Rod
Alloy No. Chemical Composition
Cu Pb Fe Fe+Sn Zn
JIS C3771 57.0~61.0 1.0~2.5 1.0 max Rem
ASTM C37700 58.0~61.0 1.5~2.5 0.30 max Rem
CW614N 57.0~59.0 1.6~2.5 0.30 max Sn<0.3, Ni<0.3,Al<0.05 Rem

Mechanical Properities

Alloy No. Temper Grade Designation Diameter(mm) TENSIL
HARDNESS Remark
Strength
Kg/mm2
Elongation(%) HV
(0.5min)
HB
(10/30000)
C3501 O C3501W-O 0.5min 30min 20min      
1/2H C3501W-1/2H 0.5~12 35~45 10min      
H C3501W-H 0.5~10 43min        
C36000                
C35300                
C3601 O C3601BD-O 6~75 30min 25min      
1/2H C3601BD-1/2H 6~50 35min   95min    
H C3601BD-H 6~20 46min   130min    
C3602 F C3602BD-F
C3602BD-F
6~75 32min   75min    
C3603 O C3603BD-O 6~75 32min 20min      
1/2H C3603BD-1/2H 6~50 37min   100min    
H C3603BD-H 6~20 46min   130min    
C3604 F C3604BD-F 6~75 34min   80min    
C3712
C3771
F C3712BD-F
C3771BD-F
6min 32min 15min